Будь ласка, використовуйте цей ідентифікатор, щоб цитувати або посилатися на цей матеріал: https://er.knutd.edu.ua/handle/123456789/17048
Повний запис метаданих
Поле DCЗначенняМова
dc.contributor.authorКалафат, К. В.uk
dc.contributor.authorТаран, Н. А.uk
dc.contributor.authorПлаван, В. П.uk
dc.contributor.authorВахітова, Л. М.uk
dc.date.accessioned2021-02-02T23:17:57Z-
dc.date.available2021-02-02T23:17:57Z-
dc.date.issued2020-
dc.identifier.citationТермодеструкція нанокомпозитів полімер-наноглина у вогнезахисних інтумесцентних покриттях / К. В. Калафат, Н. А. Таран, В. П. Плаван, Л. М. Вахітова // Advanced Polymer Materials and Technologies : conference proceedings of the III International scientific conference, dedicated to the 90th anniversary of KNUTD, Kyiv, 14-15 April 2020 / red.: V. P. Plavan, I. O. Liashok, M. K. Koliada. – Kyiv : KNUTD, 2020. – P. 104-114.uk
dc.identifier.urihttps://er.knutd.edu.ua/handle/123456789/17048-
dc.description.abstractThe aim of this work is to determine the effect of organomodified montmorillonite clay and thermally expandable graphite on the mechanism of thermodestruction and the flame retardant properties of the intumescent system of ammonium polyphosphate/melamine/pentaerythritol/polymer (nanocomposite). The structure, physico-chemical and thermal properties of polymers and nanocomposites obtained from copolymers of ethylene vinyl acetate, styrene butyl acrylate, and nanomaterials – modified benzalkonium montmorillonite (MMT) and thermally expanded graphite (EG) have been investigated. It has been proved that nanoclay and nanographite in the composition of nanocomposites enhance the thermal characteristics of the original polymers. It has been established that the thermal stability of the investigated compounds increases in a number: polymer<polymer-EG<polymer-MMT<polymer-MMT-EG. It has been shown that graphite systems are characterized by low temperature swelling (<200 °C), small length of stabilization region of swelling coefficient and significant mass loss of coke residue in the temperature range of 200–400 °C. It has been determined that the main direction of the positive effect of nanographite is the barrier effect. In turn, systems with MMT are characterized by a slowing of the onset of swelling, as well as a decrease in the swelling coefficient over the entire interval of thermal destruction of the intumescent system 200–700 °С. It has been shown that polymer-MMT nanocomposites have a positive effect on the formation of a coke layer with increasing its strength, density and adhesion to metal substrates. Based on the obtained results, an intumescent basis of fire retardant paint was developed for steel structures, which can be applied to increase the limit of metal fire resistance.en
dc.languageuk-
dc.publisherKyiv National University of Technology and Design-
dc.titleТермодеструкція нанокомпозитів полімер-наноглина у вогнезахисних інтумесцентних покриттяхuk
dc.title.alternativeThermal destruction of polymer-nanoclay nanocomposites in fire-protective intumescent coatings-
dc.typeArticle-
local.contributor.altauthorKalafat, K. V.en
local.contributor.altauthorTaran, N. A.en
local.contributor.altauthorPlavan, V. P.en
local.contributor.altauthorVakhitova, L. M.en
local.conference.nameAdvanced Polymer Materials and Technologies-
local.subject.method0-
Розташовується у зібраннях:Наукові публікації (статті)
Кафедра хімічних технологій та ресурсозбереження (ХТР)
Advanced Polymer Materials and Technologies

Файли цього матеріалу:
Файл Опис РозмірФормат 
APMT_2020_P104-114.pdf526,03 kBAdobe PDFПереглянути/Відкрити


Усі матеріали в архіві електронних ресурсів захищені авторським правом, всі права збережені.